I used a water/ molasses mix in the ratio of 10/1, so there is a wide range of options here.

Photo's from a v8 timing fixture attached:

Before, during, and after..note that the brass was not destroyed, and the decal parts are still in place. Took about 10 days on the kitchen counter..

Toothbrush , soap and water to clean up. A pressure washer for bigger bits, I imagine.
__________________
Charles Fitton
Maryhill On.,
Canada

too many carriers
too many rovers
not enough time.
(and now a BSA...)
(and now a Triumph TRW...)
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Similar Threads
Thread Thread Starter Forum Replies Last Post
Rust Remover Scott Hamilton The Restoration Forum 7 07-10-12 23:39
Mk1 Ferret added to the collection of rust! oztankboy Post-war Military Vehicles 1 06-03-12 11:42
Are rust bands required with CMP rims? Dianaa The Softskin Forum 2 10-05-11 08:07
Rust Resistant CMP gjamo For Sale Or Wanted 0 17-12-05 07:34
Rust pitting jbledsoe The Restoration Forum 2 19-10-04 14:08


All times are GMT +2. The time now is 13:54.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016