Alex 60D and 70D are hardness tests for rubber as tested with a durometer.
Rubber is measured in SHORE ratings. Standard O rings are 70 Shore and harder ones are 90 shore. 60 shore would be very soft, too soft in my opinion! Would 90 shore be too hard tho and cause premature breakup? Im a hydraulics engineer so I only understand seals...!!!
__________________
BETTER TO BURN OUT THAN FADE AWAY.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 09:12.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016