Hi Darrin

I'm not one to give welding advice , but

For steel that thick , you would be best to use a 3 phase welder , or a big DC welder driven by a petrol/deisel generator , you need big amps , single phase welding is not powerful enough .

If you have a TAFE near you, you may be able to enroll in a course and use their welding gear, they usually have big WIA 3 phase welders .

Try to study the original welds on the hull .

Also, they developed a substitute hardener for the local armour plate as they could not use Tungsten or Nickel as it wasn't available in Australia at the time ?

At a guess, the Aust. armour plate would have been made by BHP ?

Mike
__________________
1940 cab 11 C8
1940 Morris-Commercial PU
1941 Morris-Commercial CS8
1940 Chev. 15cwt GS Van ( Aust.)
1942-45 Jeep salad

Last edited by Mike K; 29-11-12 at 05:00.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 08:18.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016