I am interested in the comments made about the hardening of rivets. I'm no engineer!! When I restored my 2 pounder field gun I had to remove a few rivets from the shield. These were small dome head and countersunk. I could not drill them with even the highest quality drill bits. I could not grind the heads off as they are countersunk. The only way I could remove them was to cut the dome off and heat them with an acetylene torch till they were red hot and drive them out with a slim drift. Does this mean they were of a different steel that hardens when hot. Ron
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 08:45.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016