I have used a 45 gallon drum with a lye solution..... afull perimeter stainless steel plate with a 10 amp battery charger and two 12 volts truck batteries....... batteries went flat in a 2 hours and charger overheated......... it was really bubbling and cleaned a suspended cast CMP axles inside and out in 2 hours...... heavy scumof oil and paint on the surface.

Pressure washed and sun dried it looked like new.

Not sure how many amps were going in or how we could measure based on plate size .........

What is it in molasses that does the derusting...... the potassium content??? and if so would not a weak potassium acid bath be cheaper, faster, less sticky and stinky without being lethal to the environment?????

Bob C
__________________
Bob Carriere....B.T.B
C15a Cab 11
Hammond, Ontario
Canada
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump

Similar Threads
Thread Thread Starter Forum Replies Last Post
Rust Remover Scott Hamilton The Restoration Forum 7 07-10-12 23:39
Mk1 Ferret added to the collection of rust! oztankboy Post-war Military Vehicles 1 06-03-12 11:42
Are rust bands required with CMP rims? Dianaa The Softskin Forum 2 10-05-11 08:07
Rust Resistant CMP gjamo For Sale Or Wanted 0 17-12-05 07:34
Rust pitting jbledsoe The Restoration Forum 2 19-10-04 14:08


All times are GMT +2. The time now is 16:53.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016