Uhh just a minor invasion, thank you for asking

Yes as you've pointed out, rotary wire brushing is slow, I should have mentioned that. I've been doing my Weasel hull with it and it is indeed taking a while. I just do a square metre or two and then prime it. But for small items it's quite a reasonable sandblasting substitute which leaves the brushed surface nice and polished without pitting, and for thin panels there's no heat distortion.

Steve.
Reply With Quote
 


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 08:56.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016