Default Zinc Phosphate

Hi Colin

Zinc Phosphate I take it you are using the industrial coating type that is applied hot or hot dipped? Not the automotive metal prep.

Reason I'm asking that since basically all use gasoline has 10-15% ethanol it is playing havoc with many of the traditional gas tank coatings. It also tends to make tanks that have never rusted before rust.

So I'm trying to figure out how to make new tanks for the CMP last. Interestingly the tanks on the C60L Pat 12 built in 1941 is just mild steel, as is the C60S Pat 13 built in 1942. But my HUP tanks appear to be lead coated both inside and out.

Thanks for permission to use the photos.

Cheers Phil
__________________
Phil Waterman
`41 C60L Pattern 12
`42 C60S Radio Pattern 13
`45 HUP
http://canadianmilitarypattern.com/
New e-mail Philip@canadianmilitarypattern.com
Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 10:38.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016