Materials:

Ideally (as early prewar Carriers) Manganese Steel would be use, however this is very machining intensive - read costly.

During the war they used MCI which today has been superseeded by what is known as S.G. (Spheroidal Graphite) and is ever so easy to cast, my dad does at least two melts per week, just a little heat treatment and it's ready to be machined. It has mechanical properties very similar to Steel.

You may have read that I have just aquired two Loyd Carrier wrecks, as such I will have to be manufacturing a hell of a lot! We will need to have 8 Sprockets profiled and machined then hardened, new brake drums cast. At least I have half a set of track with them! Will keep you informed as the manufacturing process gets going.
__________________
Alastair
Lincoln, UK.


Under Restoration:
1944 No2 MK2 Loyd Carrier - Tracked Towing
1944 Ford WOT6 Lorry


The Loyd on Facebook
Reply With Quote
 

Thread Tools
Display Modes

Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT +2. The time now is 02:06.


Powered by vBulletin® Version 3.8.4
Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright © Maple Leaf Up, 2003-2016