			#1  
			
			
			
			
			
		 
		
	 | 
|||
		
		
  | 
|||
| 
		
	
		
		
			
			 
			
			Rust pitting on armoured plate...........What's the general consensus? Leave as a mark of the vehicle's history / past........Use great quantities of filler to produce that production line finish !!! 
		
		
		
		
		
		
		
		
	
	Many Thanks........ Jeff PS Still tracking down T16 parts if anyone has any offers.........  | 
| 
		 
			 
			#2  
			
			
			
			
			
		 
		
	 | 
||||
		
		
  | 
||||
| 
		
	
		
		
			
			 
			
			Depending upon the degree of pitting that you have, there is a product here in Canada which is commonly used called hi-fill or hi-solids primer. The intent of this product is to build up thickness, almost a spray Bondo if you will, that is very easy to sand and can almost be "run" to fill in imperfections. It can be applied at a very heavy rate and is very good. It can be applied in several layers to get what you need.
		 
		
		
		
		
		
		
		
		
	
	 | 
| 
		 
			 
			#3  
			
			
			
			
			
		 
		
	 | 
||||
		
		
  | 
||||
| 
		
	
		
		
			
			 Quote: 
	
 Good luck with the restoration, share some pics with us sometime eh?! Hanno  | 
![]()  | 
	
	
		
  | 
	
		
  |