Questions about the paint
Hi Tony
"So it is spot on. What I am a bit ticked off about is the semi gloss finish 'cause we also worked on getting a flat to matt finish. The spec's sent to the paint maker specified that 20% flattening agent was required. Anyway I'll work on that."
Whose paint did you use?
Did you add any hardener or other additive other than the flatten-er?
Did you get all the mixture numbers so it can be reproduced?
Reason I ask is did a similar process on my HUP and the finial coat just did not flatten the way I wanted. The problems in my case are technique and adding hardener to Enamel.
Cheers Phil
|