I started production of a 3.8 litre jar of Zinc Electroplating Solution this morning. It should be ready for the weekend in about 4 hours.

Surprisingly straightforward setup and the Cathode is bubbling merrily away as expected.

The final cleaning solution recommended for the parts to be plated after all dirt, oil and rust has been removed, is a mild solution of Hydrochloric Acid. Much easier these days to head down to the local building supply store and purchase a jug of Muriatic Acid. Same product, but a ‘commercial’ grade, as opposed to the much more expensive ‘laboratory’ grade stuff.