my thoughts were to make a resin patern by using an actual link, i got pointed in the direction of a casting compound which you pour in two stages, it then sets into hard rubber, you then remove the link and pour in the resin compound and voila.

to answer your question AJ, yes it is manganese steel. i could get a link CAD'd but it would take a millenium to do it, a laser profiler would be better, just set the link up and the machine plots it into the system by passing lasers all over the link......would cost a bomb to do it though.
__________________
is mos redintegro

__5th Div___46th Div__
1942 Ford Universal Carrier No.3 MkI*
Lower Hull No. 10131
War Department CT54508 (SOLD)
1944 Ford Universal Carrier MkII* (under restoration).
1944 Morris C8 radio body (under restoration).
Reply With Quote